  铁皮字是焊接的方式
  Iron lettering is a way of welding
  1. 氩弧焊,焊缝及焊点比较小,,比较适合薄板焊接。电流调小一点,气瓶还要有减压表,表安装到气瓶上,开的瞬间看表左边的玻璃管内的小球被吹到中间位置,(气瓶内要有气)然后焊机这边地线搭上,拿上焊把上面有个开关,焊把前端中间有个钨极,靠近焊件大概一到两毫米左右时按下开关,就会发火了,根据焊的东西厚薄调节适当的电流
  1. For argon arc welding, the welding seam and welding spot are relatively small, which is suitable for thin plate welding. Turn the current down a little, and the gas cylinder needs to have a pressure relief gauge. When the meter is installed on the gas cylinder, it can be seen that the ball in the glass tube on the left side of the meter is blown to the middle position (there should be gas in the gas cylinder). Then, the ground wire of the welding machine is connected, and there is a switch on the top of the welding handle. There is a tungsten electrode in the middle of the front end of the welding handle. When the switch is about one to two millimeters close to the weldment, it will ignite Adjust the proper current for the thickness of the welding object
            济南发光字
  2.锡焊。可以选择适合锌和铁焊接的低温焊料,比如WEWELDING M51的焊料,辅助M51-F的助焊剂焊接,焊接工作熔点温度179度的,可以通过液化气喷枪和电烙铁焊接,母体温度可以上来是关键,温度上来以后,用焊丝沾焊剂涂于焊接部位,完全靠母体热传导熔化沾有焊剂的焊丝熔化成型。
  2. Soldering. Low temperature solder suitable for zinc and iron welding can be selected, such as welding M51 solder is used to assist the flux welding of m51-f. if the welding melting point temperature is 179 ℃, it can be welded by LPG spray gun and electric soldering iron. The key is that the mother temperature can be raised. After the temperature rises, apply the welding wire with flux to the welding part, and melt the welding wire with flux completely by the heat conduction of the matrix.
  3.二保焊,铁皮厚度在2mm以上 二保焊就能完成任务,工艺大致定位 电压22V 电流100a 在这个基础上熔深较好。
  3. The second welding can complete the task if the thickness of iron sheet is more than 2 mm. The positioning voltage is 22V and the current is 100A. On this basis, the penetration is better.